Sinterlangan NdFeB magnit
Sinterlangan NdFeB magnitining jismoniy xususiyatlari | ||||||||
Baho | Remanentlik | Rev. Temp.- Koef. Of Br | Majburiy kuch | Ichki majburlash kuchi | Rev. Temp.- Koef. Hcj | Maks. Energiya mahsuloti | Maks. Ishlash harorati | Zichlik |
Br (KGs) | Hcb (SIZ) | Hcj (SIZ) | (BH) maks. (MGOe) | g/sm³ | ||||
N35 | 11.7-12.2 | -0,11~-0,12 | ≥10,9 | ≥12 | -0,58~-0,78 | 33-36 | 80℃ | 7.6 |
N38 | 12.2-12.5 | -0,11~-0,12 | ≥11,3 | ≥12 | -0,58~-0,78 | 36-39 | 80℃ | 7.6 |
N40 | 12,5-12,8 | -0,11~-0,12 | ≥11,5 | ≥12 | -0,58~-0,78 | 38-41 | 80℃ | 7.6 |
N42 | 12.8-13.2 | -0,11~-0,12 | ≥11,5 | ≥12 | -0,58~-0,78 | 40-43 | 80℃ | 7.6 |
N45 | 13.2-13.8 | -0,11~-0,12 | ≥11,6 | ≥12 | -0,58~-0,78 | 43-46 | 80℃ | 7.6 |
N48 | 13.8-14.2 | -0,11~-0,12 | ≥11,6 | ≥12 | -0,58~-0,78 | 46-49 | 80℃ | 7.6 |
N50 | 14,0-14,5 | -0,11~-0,12 | ≥10,0 | ≥12 | -0,58~-0,78 | 48-51 | 80℃ | 7.6 |
N52 | 14.3-14.8 | -0,11~-0,12 | ≥10,0 | ≥12 | -0,58~-0,78 | 50-53 | 80℃ | 7.6 |
N33M | 11.3-11.7 | -0,11~-0,12 | ≥10,5 | ≥14 | -0,58~-0,72 | 31-33 | 100℃ | 7.6 |
N35M | 11.7-12.2 | -0,11~-0,12 | ≥10,9 | ≥14 | -0,58~-0,72 | 33-36 | 100℃ | 7.6 |
N38M | 12.2-12.5 | -0,11~-0,12 | ≥11,3 | ≥14 | -0,58~-0,72 | 36-39 | 100℃ | 7.6 |
N40M | 12,5-12,8 | -0,11~-0,12 | ≥11,6 | ≥14 | -0,58~-0,72 | 38-41 | 100℃ | 7.6 |
N42M | 12.8-13.2 | -0,11~-0,12 | ≥12,0 | ≥14 | -0,58~-0,72 | 40-43 | 100℃ | 7.6 |
N45M | 13.2-13.8 | -0,11~-0,12 | ≥12,5 | ≥14 | -0,58~-0,72 | 43-46 | 100℃ | 7.6 |
N48M | 13.6-14.3 | -0,11~-0,12 | ≥12,9 | ≥14 | -0,58~-0,72 | 46-49 | 100℃ | 7.6 |
N50M | 14,0-14,5 | -0,11~-0,12 | ≥13,0 | ≥14 | -0,58~-0,72 | 48-51 | 100℃ | 7.6 |
N35H | 11.7-12.2 | -0,11~-0,12 | ≥10,9 | ≥17 | -0,58~-0,70 | 33-36 | 120 ℃ | 7.6 |
N38H | 12.2-12.5 | -0,11~-0,12 | ≥11,3 | ≥17 | -0,58~-0,70 | 36-39 | 120 ℃ | 7.6 |
N40H | 12,5-12,8 | -0,11~-0,12 | ≥11,6 | ≥17 | -0,58~-0,70 | 38-41 | 120 ℃ | 7.6 |
N42H | 12.8-13.2 | -0,11~-0,12 | ≥12,0 | ≥17 | -0,58~-0,70 | 40-43 | 120 ℃ | 7.6 |
N45H | 13.2-13.6 | -0,11~-0,12 | ≥12.1 | ≥17 | -0,58~-0,70 | 43-46 | 120 ℃ | 7.6 |
N48H | 13.7-14.3 | -0,11~-0,12 | ≥12,5 | ≥17 | -0,58~-0,70 | 46-49 | 120 ℃ | 7.6 |
N35SH | 11.7-12.2 | -0,11~-0,12 | ≥11,0 | ≥20 | -0,56~-0,70 | 33-36 | 150 ℃ | 7.6 |
N38SH | 12.2-12.5 | -0,11~-0,12 | ≥11,4 | ≥20 | -0,56~-0,70 | 36-39 | 150 ℃ | 7.6 |
N40SH | 12,5-12,8 | -0,11~-0,12 | ≥11,8 | ≥20 | -0,56~-0,70 | 38-41 | 150 ℃ | 7.6 |
N42SH | 12.8-13.2 | -0,11~-0,12 | ≥12,4 | ≥20 | -0,56~-0,70 | 40-43 | 150 ℃ | 7.6 |
N45SH | 13.2-13.8 | -0,11~-0,12 | ≥12,6 | ≥20 | -0,56~-0,70 | 43-46 | 150 ℃ | 7.6 |
N28UH | 10.2-10.8 | -0,11~-0,12 | ≥9,6 | ≥25 | -0,52~-0,70 | 26-29 | 180 ℃ | 7.6 |
N30UH | 10.8-11.3 | -0,11~-0,12 | ≥10,2 | ≥25 | -0,52~-0,70 | 28-31 | 180 ℃ | 7.6 |
N33UH | 11.3-11.7 | -0,11~-0,12 | ≥10,7 | ≥25 | -0,52~-0,70 | 31-34 | 180 ℃ | 7.6 |
N35UH | 11.8-12.2 | -0,11~-0,12 | ≥10,8 | ≥25 | -0,52~-0,70 | 33-36 | 180 ℃ | 7.6 |
N38UH | 12.2-12.5 | -0,11~-0,12 | ≥11,0 | ≥25 | -0,52~-0,70 | 36-39 | 180 ℃ | 7.6 |
N40UH | 12,5-12,8 | -0,11~-0,12 | ≥11,3 | ≥25 | -0,52~-0,70 | 38-41 | 180 ℃ | 7.6 |
N28EH | 10.4-10.9 | -0,105~-0,120 | ≥9,8 | ≥30 | -0,48~-0,70 | 26-29 | 200 ℃ | 7.6 |
N30EH | 10.8-11.3 | -0,105~-0,120 | ≥10,2 | ≥30 | -0,48~-0,70 | 28-31 | 200 ℃ | 7.6 |
N33EH | 11.3-11.7 | -0,105~-0,120 | ≥10,5 | ≥30 | -0,48~-0,70 | 31-34 | 200 ℃ | 7.6 |
N35EH | 11.7-12.2 | -0,105~-0,120 | ≥11,0 | ≥30 | -0,48~-0,70 | 33-36 | 200 ℃ | 7.6 |
N38EH | 12.2-12.5 | -0,105~-0,120 | ≥11,3 | ≥30 | -0,48~-0,70 | 36-39 | 200 ℃ | 7.6 |
N28AH | 10.4-10.9 | -0,105~-0,120 | ≥9,9 | ≥33 | -0,45~-0,70 | 26-29 | 230 ℃ | 7.6 |
N30AH | 10.8-11.3 | -0,105~-0,120 | ≥10,3 | ≥33 | -0,45~-0,70 | 28-31 | 230 ℃ | 7.6 |
N33AH | 11.3-11.7 | -0,105~-0,120 | ≥10,6 | ≥33 | -0,45~-0,70 | 31-34 | 230 ℃ | 7.6 |
Eslatma: · 20 ℃ ± 2 ℃ ish haroratida magnit kuchning muqarrar ravishda yo'qolishi 5% dan ko'p bo'lmagan magnit parametrlar va jismoniy xususiyatlar sinovdan o'tkaziladi. · Magnitning maksimal ish harorati uzunligi va diametri va atrof-muhit omillari nisbati tufayli o'zgaradi. . |
Afzallik:
Ushbu magnitlarning xususiyatlari an'anaviylardan ancha ustundir va ular hozirda qo'llashda eng kuchli hisoblanadi. Ularning balandligi
Majburiylik va yuqori turg'unlik yangi dizaynga va bo'sh joy cheklangan joylarda qo'llashning magnit maydonini oshirish imkoniyatiga imkon beradi.
yoki kuchli magnit maydon kerak bo'lganda.
NdFeB magnitlari korroziyaga juda moyil. Shuning uchun himoya sirt qoplamasi talab qilinadi. NdFeB magnitidan foydalanish shartli
80ºC dan 230ºC gacha bo'lgan keng diapazondagi harorat bilan. Shuningdek, u 0℃ dan past haroratda ishlaydi.
Ilova:
Neodimiyum magnitlari elektron, tormoz tizimlarida fokuslash, zaryadlangan zarrachalarni burish uchun turli xil magnit linzalar sifatida ishlatiladi.
tomchilatib, datchik, rotor va mikromotorlarda magnit tizim va fan sohasi, tibbiyot (tomografiya, NMR spektrometrlari) va boshqalar.
Bugungi kunda NdFeB magnitlari butun dunyoda ko'p miqdorda qo'llaniladi. Ushbu materialni ishlab chiqish hali tugallanmagan; qoldiqlik
va majburiy maydon kuchi doimiy ravishda oshirilmoqda. NdFeB magnitlarining yuqori energiyasi motorlar va sensorlarni qurish mumkinligini anglatadi
har doim kichikroq - va bu ishlash samaradorligini oshirishni bildiradi. Doimiy yaxshilanishlar ushbu qiziqarli materialni davom ettirishga imkon beradi.
har yili yangi hududlarga kiritiladi.
Barcha ko'rsatilgan qiymatlar IEC 60404-5 ga muvofiq standart namunalar yordamida aniqlangan. Quyidagi spetsifikatsiyalar mos yozuvlar qiymatlari sifatida xizmat qiladi va
farq qilishi mumkin. Qo'shimcha ma'lumot olish uchun ilova muhandislarimiz bilan bog'laning.